SKY-A2 Zirconium silicate

Alternative and trade names
SKY-A2
Want to keep this datasheet? Save it now in your required format

Description

Non-toxic and tasteless white powder with stable chemical properties. The specific surface area can be controlled.

This material data has been provided by Zhengzhou Sky Universe Trade Co.,LTD..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

4.56 g/cm³

Show Supplier Material materials with Density of 4.56 g/cm³

Particle size D50

0.8 - 0.9 μm

Show Supplier Material materials with Particle size D50 of 0.8 - 0.9 μm

Chemical properties

PropertyValueComment

Iron

0.1 %

Show Supplier Material materials with Iron of 0.1 %

Fe₂O₃

Titanium

0.15 %

Show Supplier Material materials with Titanium of 0.15 %

TiO₂

Zirconium

64.5 - 65.5 %

Show Supplier Material materials with Zirconium of 64.5 - 65.5 %

ZrO₂

Technological properties

Property
Application areas

Plastic industry,Refractory materials,as emulsifying agent used in various types of ceramic glaze,coffee cups for export,sanitary ceramics,floor tiles,building tiles.It also can be used in making ceramics rollers and brake discs. Used for epoxy resin formulations,the sealing resin,silicones,vinyl resins,and as the filler material of resin in order to increase the heat resistance and improve the insulation value and it also used in filler materials that requires inert, fine, white and chemical resistant. Casted refractories for glass melting furnaces, heat resistant porcelain, sand flushing in refractory casting and the refractory slabs, special fire resistant porcelain, refractory cement.