Dimension
Property | Value |
---|---|
Diameter | 25.4 - 355.6 mm Show Supplier Material materials with Diameter of 25.4 - 355.6 mm |
Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 23.0 °C | 8 % Show Supplier Material materials with Elongation of 8 % |
Hardness, Brinell | 23.0 °C | 388 [-] Show Supplier Material materials with Hardness, Brinell of 388 [-] |
Tensile strength | 23.0 °C | 1310 MPa Show Supplier Material materials with Tensile strength of 1310 MPa |
Yield strength Rp0.2 | 23.0 °C | 1170 MPa Show Supplier Material materials with Yield strength Rp0.2 of 1170 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Carbon | 0.07 % Show Supplier Material materials with Carbon of 0.07 % | ||
Chromium | 15 - 17.5 % Show Supplier Material materials with Chromium of 15 - 17.5 % | ||
Copper | 3 - 5 % Show Supplier Material materials with Copper of 3 - 5 % | ||
Iron | Balance | ||
Manganese | 1 % Show Supplier Material materials with Manganese of 1 % | ||
Nickel | 3 - 5 % Show Supplier Material materials with Nickel of 3 - 5 % | ||
Other | 0.15 - 0.45 % Show Supplier Material materials with Other of 0.15 - 0.45 % | Nb+Ta | |
Phosphorus | 0.04 % Show Supplier Material materials with Phosphorus of 0.04 % | ||
Silicon | 1 % Show Supplier Material materials with Silicon of 1 % | ||
Sulfur | 0.03 % Show Supplier Material materials with Sulfur of 0.03 % |
Technological properties
Property | ||
---|---|---|
Application areas | chemical, petrochemical, paper and general metalworking industries | |
Heat Treatment | Solution annealing at 1000 to 1050°C, hardened at 480°C | |
Welding | Good, Pre-heating and post-heating practices used for standard hardenable stainless grades are not required. Min. RREN: 17 |