EDX 2304 L Profile

Alternative and trade names
EDX 2304, ALLOY 1.4362, LEAN DUPLEX UNS S32304
Want to keep this datasheet? Save it now in your required format

Description

EDX 2304 according to MDS D35 has an improved balanced chemistry of chromium, molybdenum and nitrogen. Increased mechanical strength compared to the standard UNS 32304. EDX 2304 outruns both 1.4404 and 1.4436 with respect to pitting corrosion resistance. Due to risk of embrittlement, duplex steels should not be used at temperatures above 250 – 325°C.

Related Standards

Equivalent Materials

This material data has been provided by Sverdrup Steel.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Thickness

5 - 10 mm

Show Supplier Material materials with Thickness of 5 - 10 mm

Width

50 - 100 mm

Show Supplier Material materials with Width of 50 - 100 mm

Mechanical

PropertyTemperatureValueComment

Charpy impact energy, V-notch

-46.0 °C

45 J

Show Supplier Material materials with Charpy impact energy, V-notch of 45 J

Elongation

23.0 °C

25 %

Show Supplier Material materials with Elongation of 25 %

Hardness, Brinell

23.0 °C

290 [-]

Show Supplier Material materials with Hardness, Brinell of 290 [-]

Tensile strength

23.0 °C

630 MPa

Show Supplier Material materials with Tensile strength of 630 MPa

Yield strength Rp0.2

23.0 °C

500 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 500 MPa

T<13MM

Chemical properties

PropertyValue

Carbon

0.03 %

Show Supplier Material materials with Carbon of 0.03 %

Chromium

22 - 24 %

Show Supplier Material materials with Chromium of 22 - 24 %

Copper

0.1 - 0.6 %

Show Supplier Material materials with Copper of 0.1 - 0.6 %

Iron

Balance

Manganese

2 %

Show Supplier Material materials with Manganese of 2 %

Molybdenum

0.1 - 0.6 %

Show Supplier Material materials with Molybdenum of 0.1 - 0.6 %

Nickel

3.5 - 5.5 %

Show Supplier Material materials with Nickel of 3.5 - 5.5 %

Nitrogen

0.05 - 0.2 %

Show Supplier Material materials with Nitrogen of 0.05 - 0.2 %

Other

B: 35 PPM

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

Silicon

1 %

Show Supplier Material materials with Silicon of 1 %

Sulfur

0.015 %

Show Supplier Material materials with Sulfur of 0.015 %

Technological properties

Property
Application areas

The main applications are for details with special requirements for high corrosion resistance.

Corrosion properties

Good resistance to stress corrosion cracking, Good resistance to pitting and crevice corrosion, High resistance to general corrosion, High resistance to erosion corrosion and corrosion fatigue. PREN ≥ 28

Heat Treatment

Solution annealing at 1020 – 1100°C followed by water quenching

Welding

Very good