Dimension
Property | Value |
---|---|
Diameter | 10 - 300 mm Show Supplier Material materials with Diameter of 10 - 300 mm |
Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 23.0 °C | 20 % Show Supplier Material materials with Elongation of 20 % |
Hardness, Rockwell B | 23.0 °C | 160 [-] Show Supplier Material materials with Hardness, Rockwell B of 160 [-] |
Tensile strength | 23.0 °C | 345 MPa Show Supplier Material materials with Tensile strength of 345 MPa |
Yield strength Rp0.2 | 23.0 °C | 276 - 448 MPa Show Supplier Material materials with Yield strength Rp0.2 of 276 - 448 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.08 % Show Supplier Material materials with Carbon of 0.08 % |
Hydrogen | 0.02 % Show Supplier Material materials with Hydrogen of 0.02 % |
Iron | 0.3 % Show Supplier Material materials with Iron of 0.3 % |
Nitrogen | 0.03 % Show Supplier Material materials with Nitrogen of 0.03 % |
Oxygen | 0.25 % Show Supplier Material materials with Oxygen of 0.25 % |
Titanium | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | Grade 2 titanium is also used to manufacture heat exchangers and cryogenic vessels. In seawater, Grade 2 is fully resistant to corrosion at temperatures up to 300°C. | |
Corrosion properties | It is highly resistant to chemical environments including oxidizing media, alkaline media, organic acids and compounds, aqueous salt solutions and hot gases. Its corrosion resistance holds up in liquid metals, nitric acid, mildly reducing acids and wet chlorine or bromine gas. |