Low Alloy Steel

Customize your search with filters

Material Supplied by

Sverdrup Steel AS

AISI 4130 MODIFIED Quenched & Tempered Tube

Alternative and trade names
EN 1.7220, UNS G41300, ASTM 4130
.XLSX
.PDF
Save

Description

AISI 4130 is a low alloy C-steel containing chromium and molybdenum as strengthening agents. It has low carbon content, and hence it can be welded easily. It is supplied as round bar commonly in the hardened and tempered condition with a hardness of 18-22 HRc.

Related standards

Properties

Dimension

Diameter d

130 - 304.8 mm

Mechanical

Elongation A

17 - 18 % at 20 °C

Hardness, Rockwell C HRC

22 [-] at 20 °C

Impact strength, Charpy notched Ivnot

42 kJ/m² at -32 °C

Tensile strength Rm

585 - 655 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

414 - 517 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cr

0.8 - 1.1 %

Mn

0.4 - 0.6 %

C

0.28 - 0.33 %

Mo

0.15 - 0.25 %

Si

0.15 - 0.35 %

More

Technological properties

Application areas

AISI 4130 is a low alloyed hardened and tempered steel used for Oil and gas drilling and production equipment – wellhead and Christmas tree equipment.

Processing history

Hardened at 860°C followed by water quenching. Tempering at min. 650°C, cooled in air.

Welding