General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 7.93 g/cm³ Show Supplier Material materials with Density of 7.93 g/cm³ |
Mechanical
Chemical properties
Property | Value |
---|---|
Carbon | 0.08 % Show Supplier Material materials with Carbon of 0.08 % |
Chromium | 17 - 19 % Show Supplier Material materials with Chromium of 17 - 19 % |
Manganese | 2 % Show Supplier Material materials with Manganese of 2 % |
Nickel | 9 - 12 % Show Supplier Material materials with Nickel of 9 - 12 % |
Phosphorus | 0.05 % Show Supplier Material materials with Phosphorus of 0.05 % |
Silicon | 0.75 % Show Supplier Material materials with Silicon of 0.75 % |
Sulfur | 0.03 % Show Supplier Material materials with Sulfur of 0.03 % |
Technological properties
Property | ||
---|---|---|
Application areas | Pressure Vessel& Anti-Corrosion Building |