General
Property | Value | Comment |
---|---|---|
Lateral flake size | 26500.0 Show Supplier Material materials with Lateral flake size of 26500.0 | Using SEM |
Layer number | 1.0 - 100.0 [-] Show Supplier Material materials with Layer number of 1.0 - 100.0 [-] | ≤5 is 18%, ≤10 is 73% and 10-100 is 27%, using Raman |
Chemical properties
Property | Value |
---|---|
Carbon | 93.0 - 99.0 % Show Supplier Material materials with Carbon of 93.0 - 99.0 % |
Fluorine | 2.0 % Show Supplier Material materials with Fluorine of 2.0 % |
Nitrogen | 0.6000000000000001 % Show Supplier Material materials with Nitrogen of 0.6000000000000001 % |
Oxygen | 1.0 - 5.0 % Show Supplier Material materials with Oxygen of 1.0 - 5.0 % |
Sulfur | 2.0 % Show Supplier Material materials with Sulfur of 2.0 % |
Technological properties
Property | ||
---|---|---|
Application areas | Being electrically conductive, thermally conductive and a highly effective mechanical reinforcer there are numerous potential applications for graphene such as: composites, energy, biomedical, membranes, coatings, sensors, electronics |