In addition to our high quality, low defect graphene powders, we also supply reduced graphene oxide. With a higher defect ratio, these products are suitable for different applications where the high proportion of oxygen would be beneficial.
Lateral flake size
wFlake20000 nm
Using SEM/AFM
Layer number
nLayer1 - 100 [-]
Using AFM
Element
Weight %
Comment
87.5 - 92.5 %
4.5 - 19.5 %
0 - 3 %
0 - 5 %
0 - 3 %
Application areas
li-ion batteries, fuel cells, battery electrodes, solar pv cells, electrically conductive inks, thermally conductive films and coatings, thermal interface materials, lightweight composites, concrete, metal -matrix composites, corrosion protection, barrier properties / permeation / mechanical performance.
Color
Black
This material data has been provided by Versarien.