Description

In addition to our high quality, low defect graphene powders, we also supply reduced graphene oxide. With a higher defect ratio, these products are suitable for different applications where the high proportion of oxygen would be beneficial.

This material data has been provided by Versarien.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Lateral flake size

20000.0

Show Supplier Material materials with Lateral flake size of 20000.0

Using SEM/AFM

Layer number

1.0 - 100.0 [-]

Show Supplier Material materials with Layer number of 1.0 - 100.0 [-]

Using AFM

Chemical properties

PropertyValue

Carbon

87.5 - 92.5 %

Show Supplier Material materials with Carbon of 87.5 - 92.5 %

Manganese

3.0 %

Show Supplier Material materials with Manganese of 3.0 %

Nitrogen

5.0 %

Show Supplier Material materials with Nitrogen of 5.0 %

Oxygen

4.5 - 19.5 %

Show Supplier Material materials with Oxygen of 4.5 - 19.5 %

Sulfur

3.0 %

Show Supplier Material materials with Sulfur of 3.0 %

Technological properties

Property
Application areas

li-ion batteries, fuel cells, battery electrodes, solar pv cells, electrically conductive inks, thermally conductive films and coatings, thermal interface materials, lightweight composites, concrete, metal -matrix composites, corrosion protection, barrier properties / permeation / mechanical performance.

Color