ASTM Grade 2 Tube

Supplied by Vero Specialty Metals
Contact supplier
Vero Specialty Metals
View full profile

Chemical composition

Element Weight %
Ti
bal
Fe 0.3
O 0.25
C 0.1
N 0.03
H 0.0125

Properties

General information

Density [ ρ ]

4.51 g/cm³

Mechanical

Elastic modulus [ E ]

110.00 GPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
This material data has been provided by Vero Specialty Metals.