Titanium Grade 9 (Ti-3Al-2,5V) Plate

.XLSX
.PDF
Save

Description

Equivalent Materials

Ashby charts

Properties

General

Density ρ

4.48 g/cm³ at 20 °C

Dimension

Length l

1500 - 6500 mm

Thickness t

4.76 - 200 mm

Width w

600 - 1600 mm

Mechanical

Elastic modulus E

103 GPa at 20 °C

Elongation A5 A5

15 % at 20 °C

Tensile strength Rm

620 MPa at 20 °C

Yield strength YS

520 MPa at 20 °C

Thermal

Thermal conductivity λ

8.3 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Al

3 %

V

2.5 %