General
Property | Value | Shape |
---|---|---|
Density | 4.5 g/cm³ Show Material materials with Density of 4.5 g/cm³ | Sheet, Plate |
Dimension
Property | Value | Shape |
---|---|---|
Length | 1500 mm Show Material materials with Length of 1500 mm | Sheet, Plate |
5000 mm Show Material materials with Length of 5000 mm | Sheet | |
6500 mm Show Material materials with Length of 6500 mm | Plate | |
Width | 400 mm Show Material materials with Width of 400 mm | Sheet |
600 mm Show Material materials with Width of 600 mm | Plate | |
1524 mm Show Material materials with Width of 1524 mm | Sheet | |
1600 mm Show Material materials with Width of 1600 mm | Plate |
valueMetaData
Property | Value |
---|
Mechanical
Property | Value | Shape |
---|---|---|
Elastic modulus | 105.0 GPa Show Material materials with Elastic modulus of 105.0 GPa | Sheet, Plate |
Hardness, Brinell | 170.0 Show Material materials with Hardness, Brinell of 170.0 | Sheet, Plate |
Tensile strength | 480.0 MPa Show Material materials with Tensile strength of 480.0 MPa | Sheet, Plate |
Yield strength | 345.0 MPa Show Material materials with Yield strength of 345.0 MPa | Sheet, Plate |
Thermal
Property | Value | Shape | Comment |
---|---|---|---|
Coefficient of thermal expansion | 7.599999999999997e-06 - 1.1e-05 1/K Show Material materials with Coefficient of thermal expansion of 7.599999999999997e-06 - 1.1e-05 1/K | Typical for Titanium Near Alpha Alloy | |
Melting point | 1540.0 - 1715.0 °C Show Material materials with Melting point of 1540.0 - 1715.0 °C | Typical for Titanium Near Alpha Alloy | |
Specific heat capacity | 520 J/(kg·K) Show Material materials with Specific heat capacity of 520 J/(kg·K) | Sheet, Plate | |
Thermal conductivity | 22.6 W/(m·K) Show Material materials with Thermal conductivity of 22.6 W/(m·K) | Sheet, Plate |
Chemical properties
Property | Value | Shape |
---|---|---|
Carbon | 0.08 Show Material materials with Carbon of 0.08 | Sheet, Plate |
Hydrogen | 0.015 Show Material materials with Hydrogen of 0.015 | Sheet, Plate |
Iron | 0.3 Show Material materials with Iron of 0.3 | Sheet, Plate |
Molybdenum | 0.2 - 0.4 % Show Material materials with Molybdenum of 0.2 - 0.4 % | Sheet, Plate |
Nickel | 0.6 - 0.9 % Show Material materials with Nickel of 0.6 - 0.9 % | Sheet, Plate |
Nitrogen | 0.03 Show Material materials with Nitrogen of 0.03 | Sheet, Plate |
Oxygen | 0.25 Show Material materials with Oxygen of 0.25 | Sheet, Plate |