General
Property | Value | Shape |
---|---|---|
Density | 4.45 g/cm³ Show Material materials with Density of 4.45 g/cm³ | Sheet, Plate |
Dimension
Property | Value | Shape |
---|---|---|
Length | 1500 mm Show Material materials with Length of 1500 mm | Sheet, Plate |
5000 mm Show Material materials with Length of 5000 mm | Sheet | |
6500 mm Show Material materials with Length of 6500 mm | Plate | |
Width | 400 mm Show Material materials with Width of 400 mm | Sheet |
600 mm Show Material materials with Width of 600 mm | Plate | |
1524 mm Show Material materials with Width of 1524 mm | Sheet | |
1600 mm Show Material materials with Width of 1600 mm | Plate |
valueMetaData
Property | Value |
---|
Mechanical
Property | Value | Shape |
---|---|---|
Elastic modulus | 110.0 GPa Show Material materials with Elastic modulus of 110.0 GPa | Sheet, Plate |
Tensile strength | 825.0 - 860.0 MPa Show Material materials with Tensile strength of 825.0 - 860.0 MPa | Sheet, Plate |
Yield strength | 760.0 MPa Show Material materials with Yield strength of 760.0 MPa | Sheet, Plate |
Thermal
Property | Value | Shape | Comment |
---|---|---|---|
Coefficient of thermal expansion | 7.699999999999999e-06 - 1e-05 1/K Show Material materials with Coefficient of thermal expansion of 7.699999999999999e-06 - 1e-05 1/K | Typical for Titanium Alpha Beta Alloy | |
Melting point | 1500.0 - 1750.0 °C Show Material materials with Melting point of 1500.0 - 1750.0 °C | Typical for Titanium Alpha Beta Alloy | |
Specific heat capacity | 560 J/(kg·K) Show Material materials with Specific heat capacity of 560 J/(kg·K) | Sheet, Plate | |
Thermal conductivity | 6.9 W/(m·K) Show Material materials with Thermal conductivity of 6.9 W/(m·K) | Sheet, Plate |
Chemical properties
Property | Value | Shape |
---|---|---|
Aluminium | 5.5 - 6.5 % Show Material materials with Aluminium of 5.5 - 6.5 % | Sheet, Plate |
Carbon | 0.08 Show Material materials with Carbon of 0.08 | Sheet, Plate |
Hydrogen | 0.015 Show Material materials with Hydrogen of 0.015 | Sheet, Plate |
Iron | 0.25 Show Material materials with Iron of 0.25 | Sheet, Plate |
Nitrogen | 0.05 Show Material materials with Nitrogen of 0.05 | Sheet, Plate |
Oxygen | 0.13 Show Material materials with Oxygen of 0.13 | Sheet, Plate |
Vanadium | 3.5 - 4.5 % Show Material materials with Vanadium of 3.5 - 4.5 % | Sheet, Plate |