Dimension

Length l

1500 - 6500 mm

Thickness t

4.76 - 200 mm

Width w

600 - 1600 mm

General

Density ρ

4.76 g/cm³ at 20 °C

Mechanical

Elastic modulus E

82 GPa at 20 °C

Elongation A

22 % at 20 °C

Hardness, Rockwell B HRB

95 [-] at 20 °C

Poisson's ratio ν

0.33 [-] at 20 °C

Shear modulus G

30.8 GPa at 20 °C

Tensile strength Rm

790 MPa at 20 °C

Yield strength YS

770 MPa at 20 °C

Thermal

Thermal conductivity λ

8.08 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

V

15 %

Al

3 %

H

3 %

Sn

3 %

This material data has been provided by VSMPO.