Ti-4Al-4Mo-2Sn Bar

.XLSX
.PDF
Save

Properties

Dimension

Diameter d

7 - 115 mm

Length l

6000 mm

max

General

Density ρ

4.59 g/cm³ at 20 °C

Material Information

Dimension

7-14.5 mm diameter up to 3000 mm length; 15-65 mm diameter up to 6000 mm length; 66-115 mm diameter up to 5000 mm length.

Mechanical

Elastic modulus E

114 GPa at 20 °C

Elongation A

12 % at 20 °C

Tensile strength Rm

1138 MPa at 20 °C

Yield strength YS

1035 MPa at 20 °C

Thermal

Thermal conductivity λ

7.6 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Al

3 - 5 %

Mo

3 - 5 %

Sn

1.5 - 2.5 %

Si

0.3 - 0.7 %

O

0.27 %

More

This material data has been provided by VSMPO.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.