General
Property | Value | Shape |
---|---|---|
Density | 4.48 g/cm³ Show Material materials with Density of 4.48 g/cm³ | Sheet, Billet, Tube |
Dimension
Property | Value | Shape |
---|---|---|
Diameter | 5 mm Show Material materials with Diameter of 5 mm | Tube |
25.4 mm Show Material materials with Diameter of 25.4 mm | Billet | |
125 mm Show Material materials with Diameter of 125 mm | Billet | |
130 mm Show Material materials with Diameter of 130 mm | Tube | |
Length | 1000 mm Show Material materials with Length of 1000 mm | Tube |
1500 mm Show Material materials with Length of 1500 mm | Sheet | |
5000 mm Show Material materials with Length of 5000 mm | Sheet, Tube | |
6500 mm Show Material materials with Length of 6500 mm | Sheet | |
Wall thickness | 0.5 - 9.0 mm Show Material materials with Wall thickness of 0.5 - 9.0 mm | Tube |
2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | Billet | |
Width | 400 mm Show Material materials with Width of 400 mm | Sheet |
600 mm Show Material materials with Width of 600 mm | Sheet | |
1524 mm Show Material materials with Width of 1524 mm | Sheet | |
1600 mm Show Material materials with Width of 1600 mm | Sheet |
valueMetaData
Property | Value |
---|
Mechanical
Property | Value | Shape |
---|---|---|
Elastic modulus | 103.0 GPa Show Material materials with Elastic modulus of 103.0 GPa | Sheet, Billet, Tube |
Elongation | 15.0 % Show Material materials with Elongation of 15.0 % | Billet |
Hardness, Brinell | 256.0 Show Material materials with Hardness, Brinell of 256.0 | Billet, Tube |
Hardness, Rockwell C | 24.0 [-] Show Material materials with Hardness, Rockwell C of 24.0 [-] | Billet, Tube |
Hardness, Vickers | 280.0 Show Material materials with Hardness, Vickers of 280.0 | Billet, Tube |
Poisson's ratio | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Billet, Tube |
Shear modulus | 44.0 GPa Show Material materials with Shear modulus of 44.0 GPa | Billet, Tube |
Tensile strength | 620.0 MPa Show Material materials with Tensile strength of 620.0 MPa | Sheet, Billet, Tube |
Yield strength | 520.0 MPa Show Material materials with Yield strength of 520.0 MPa | Sheet, Billet, Tube |
Thermal
Property | Value | Shape | Comment |
---|---|---|---|
Coefficient of thermal expansion | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coefficient of thermal expansion of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Titanium | |
Melting point | 1700.0 °C Show Material materials with Melting point of 1700.0 °C | Billet, Tube | |
Thermal conductivity | 8.3 W/(m·K) Show Material materials with Thermal conductivity of 8.3 W/(m·K) | Sheet, Billet, Tube |
Chemical properties