Property | Temperature | Value | Comment |
---|---|---|---|
Density | 20.0 °C | 1.02 - 1.06 g/cm³ Show Supplier Material materials with Density of 1.02 - 1.06 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 2 - 2.4 GPa Show Supplier Material materials with Elastic modulus of 2 - 2.4 GPa | ISO 527-2 |
Elongation | 20.0 °C | 9 - 11 % Show Supplier Material materials with Elongation of 9 - 11 % | ISO 527-1/-2 |
Impact strength, Charpy notched | 20.0 °C | 16 - 24 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 16 - 24 kJ/m² | ISO 179/1eA |
Impact strength, Charpy unnotched | 20.0 °C | 150 - 190 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 150 - 190 kJ/m² | ISO 179/1eA |
Tensile strength | 20.0 °C | 35 - 45 MPa Show Supplier Material materials with Tensile strength of 35 - 45 MPa | ISO 527-1/-2 |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Ash content | 20.0 °C | 2 % Show Supplier Material materials with Ash content of 2 % | Maximum |
Rheological Properties
Property | Value | Comment |
---|---|---|
Melt volume-flow rate | 14 - 24 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 14 - 24 cm³/10min | ISO 1133, 220°C/10Kg |
Technological properties
Property | ||
---|---|---|
Application areas | House trunks, Industrial trunks, Car interior cases, Seating | |
Processing methods | Pre-drying 2-4 hours/79°C |