General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 15 g/cm³ Show Material materials with Density of 15 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Flexural strength | 20.0 °C | 1034 - 1103 MPa Show Material materials with Flexural strength of 1034 - 1103 MPa |
Hardness, Rockwell B | 20.0 °C | 94 - 106 [-] Show Material materials with Hardness, Rockwell B of 94 - 106 [-] |
Tensile strength | 20.0 °C | 620 - 689 MPa Show Material materials with Tensile strength of 620 - 689 MPa |
Electrical
Property | Value |
---|---|
Specific Electrical conductivity | 25 - 45 % IACS Show Material materials with Specific Electrical conductivity of 25 - 45 % IACS |
Chemical properties
Property | Value |
---|---|
Copper | 18 - 22 % Show Material materials with Copper of 18 - 22 % |