ASTM B351 Grade R60001 soft annealed (+A)

.XLSX
.PDF
Save

Description

Hot-rolled and cold-finished zirconium bars, rod, and wire for nuclear application for nuclear application.

Related Standards

Equivalent Materials

Properties

General

Density ρ

6.6 g/cm³ at 20 °C

Mechanical

Elongation A50 A50

18 % at 20 °C

Tensile strength Rm

290 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

140 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Zr

99.5 %

This material data has been provided by WIAM.