ASTM B351 R60001 soft annealed (+A) Wire

.XLSX
.PDF
Save

Description

Primary standard name

Properties

Mechanical

Elongation A50 A50

18 % at 20 °C

Tensile strength Rm

290 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

140 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Zr

99.5 %