Properties

General

Density

ρ

2.72 g/cm³ at 20 °C

Dimension

Dimensions

Durchmesser

Thickness

t

0.3 - 1.5 mm

Mechanical

Bending angle 180°

θ180

1.5 - 2.5 °/t at 20 °C

Show 3000 Series materials with Bending angle 180° of 1.5 - 2.5 °/t at 20 °C

Bending angle 90°

θ90

0.5 - 2 °/t at 20 °C

Show 3000 Series materials with Bending angle 90° of 0.5 - 2 °/t at 20 °C

Elastic modulus

E

69 - 70 GPa at 20 °C

Show 3000 Series materials with Elastic modulus of 69 - 70 GPa at 20 °C

Elongation

A

7 % at 20 °C

Show 3000 Series materials with Elongation of 7 % at 20 °C

Elongation A100

A100

7 % at 20 °C

Show 3000 Series materials with Elongation A100 of 7 % at 20 °C

Elongation A50

A50

1 - 3 % at 20 °C

Show 3000 Series materials with Elongation A50 of 1 - 3 % at 20 °C

Elongation A50, transverse

A50,trans

1 - 3 % at 20 °C

Show 3000 Series materials with Elongation A50, transverse of 1 - 3 % at 20 °C

Hardness, Brinell

HB

54 [-] at 20 °C

Show 3000 Series materials with Hardness, Brinell of 54 [-] at 20 °C

Hardness, HBW

HBW

53 [-] at 20 °C

Show 3000 Series materials with Hardness, HBW of 53 [-] at 20 °C

Plane-Strain Fracture Toughnes

KIC

22 - 35 MPa·√m at 20 °C

Show 3000 Series materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 20 °C

Typical for Wrought 3000 Series Aluminium

Poisson's ratio

ν

0.33 [-] at 20 °C

Show 3000 Series materials with Poisson's ratio of 0.33 [-] at 20 °C

Typical for Wrought 3000 Series Aluminium

Shear modulus

G

26 - 26.5 GPa at 20 °C

Show 3000 Series materials with Shear modulus of 26 - 26.5 GPa at 20 °C

Tensile strength

Rm

170 - 215 MPa at 20 °C

Show 3000 Series materials with Tensile strength of 170 - 215 MPa at 20 °C

Tensile strength, transverse

Rm,trans

170 - 215 MPa at 20 °C

Show 3000 Series materials with Tensile strength, transverse of 170 - 215 MPa at 20 °C

Yield strength

YS

130 MPa at 20 °C

Show 3000 Series materials with Yield strength of 130 MPa at 20 °C

Yield strength Rp0.2

Rp0.2

150 - 175 MPa at 20 °C

Show 3000 Series materials with Yield strength Rp0.2 of 150 - 175 MPa at 20 °C

Yield strength Rp0.2, transverse

Rp0.2,trans

150 MPa at 20 °C

Show 3000 Series materials with Yield strength Rp0.2, transverse of 150 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

2.32E-5 1/K at 20 °C

20-100°C

Hide chart

Melting point

Tm

630 - 654 °C

Specific heat capacity

cp

893 J/(kg·K) at 20 °C

Thermal conductivity

λ

160 - 200 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

2.30E+7 - 2.80E+7 S/m at 20 °C

Electrical resistivity

ρel

3.8E-8 - 4.35E-8 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Other

-

each 0.05, total 0.15, Rest Al

Mn

1 - 1.5 %

Fe

0.7 %

Si

0.6 %

Cu

0.3 %

More

Technological properties

Anodizing

Good

Application areas

Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Electronic devices: Housing of devices; Insulation; Cosmetics: Cosmetics pieces

Brazing

Good

Corrosion properties

Good

Welding

Good

Workability

Good

This material data has been provided by Aludium,WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.