Properties

General

Density

ρ

2.7 - 2.71 g/cm³ at 20 °C

Dimension

Dimensions

Dicke

Thickness

t

0.2 - 6 mm

Mechanical

Plane-Strain Fracture Toughnes

KIC

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

ν

Typical for Wrought 5000 Series Aluminium

Tensile strength, transverse

Rm,trans

Yield strength Rp0.2, transverse

Rp0.2,trans

Thermal

Coefficient of thermal expansion

α

2.37E-5 1/K at 20 °C

20-100°C

Unlock all property charts

Max service temperature

Tmax

150 °C

Typical for Wrought 5000 Series Aluminium

Max service temperature, long

Tmaxlong

0 - 150 °C

Melting point

Tm

620 - 650 °C

Specific heat capacity

cp

879 - 963 J/(kg·K) at 20 °C

Typical for Wrought 5000 Series Aluminium

Thermal conductivity

λ

140 - 180 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

2.00E+7 - 2.50E+7 S/m at 20 °C

Electrical resistivity

ρel

4E-8 - 5E-8 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Mg

1.6 - 2.5 %

Fe

0.5 %

Mn

0.5 - 1.1 %

Si

0.4 %

Cr

0.3 %

More

Technological properties

Anodizing

Excellent (anodizing quality)

Application areas

Components: General trasportation

Brazing

Poor

Corrosion properties

Excellent

Welding

Very Good

Workability

Very Good (in O temper)

This material data has been provided by Aludium,WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.