Customize your search with filters
Do you have any questions?
Density ρ
2.8 g/cm³ at 20 °C
Elongation A
6 - 7 % at 20 °C
Elongation A50 A50
4 - 5 % at 20 °C
Tensile strength Rm
415 - 450 MPa at 20 °C
Yield strength Rp0.2 Rp0.2
370 - 400 MPa at 20 °C
Element
Weight %
Comment
3.9 - 5 %
0.5 - 0.9 %
0.5 %
0.4 - 1.2 %
0.25 %