Description

Primary standard name

Properties

Electrical

Electrical conductivity σel

1.80E+7 - 2.80E+7 S/m at 20 °C

General

Density ρ

2.79 - 2.8 g/cm³ at 20 °C

Mechanical

Elastic modulus E

65 - 73.5 GPa at 20 °C

Elongation A

10 % at 20 °C

Elongation A50 A50

8 % at 20 °C

Tensile strength Rm

380 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

260 MPa at 20 °C

Thermal

Melting point Tm

650 °C

Specific heat capacity cp

921 J/(kg·K) at 20 °C

Thermal conductivity λ

130 - 200 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

3.5 - 4.5 %

Fe

0.7 %

Mn

0.4 - 1 %

Mg

0.4 - 1 %

Zn

0.25 %

More

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.