EN AW-2030 T4 Profile

.XLSX
.PDF
Save

Description

Primary standard name

Properties

General

Density ρ

2.81 g/cm³ at 20 °C

Mechanical

Elongation A

8 % at 20 °C

Elongation A50 A50

6 % at 20 °C

Tensile strength Rm

370 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

250 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

3.3 - 4.5 %

Si

0.8 %

Pb

0.8 - 1.5 %

Fe

0.7 %

Zn

0.5 %

More

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.