General
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Density | 20.0 °C | 2.75 g/cm³ Show Material materials with Density of 2.75 g/cm³ | T5 | DIN 1725-2, EN 1676, EN 1706 |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Elastic modulus | 20.0 °C | 75.0 GPa Show Material materials with Elastic modulus of 75.0 GPa | T5 | DIN 1725-2, EN 1676, EN 1706 | |
Elongation | 220.0 °C | 8.4 % Show Material materials with Elongation of 8.4 % | T5 | DIN 1725-2, EN 1676, EN 1706 | |
280.0 °C | 21.8 % Show Material materials with Elongation of 21.8 % | T5 | DIN 1725-2, EN 1676, EN 1706 | ||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | |||
Shear modulus | 2.8 GPa Show Material materials with Shear modulus of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | |||
Tensile strength | 20.0 °C | 348.0 MPa Show Material materials with Tensile strength of 348.0 MPa | T5 | DIN 1725-2, EN 1676, EN 1706 | |
220.0 °C | 133.0 MPa Show Material materials with Tensile strength of 133.0 MPa | T5 | DIN 1725-2, EN 1676, EN 1706 | ||
280.0 °C | 66.0 MPa Show Material materials with Tensile strength of 66.0 MPa | T5 | DIN 1725-2, EN 1676, EN 1706 |
Thermal
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 200.0 °C | 2.1e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.1e-05 1/K | T5 | DIN 1725-2, EN 1676, EN 1706 | |
Melting point | 505.0 - 770.0 °C Show Material materials with Melting point of 505.0 - 770.0 °C | Typical for Cast 3xx.x Series Aluminium | |||
Specific heat capacity | 20.0 °C | 880.0 J/(kg·K) Show Material materials with Specific heat capacity of 880.0 J/(kg·K) | T5 | DIN 1725-2, EN 1676, EN 1706 | |
Thermal conductivity | 20.0 °C | 110.0 - 130.0 W/(m·K) Show Material materials with Thermal conductivity of 110.0 - 130.0 W/(m·K) | T5 | DIN 1725-2, EN 1676, EN 1706 |
Electrical
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Electrical conductivity | 20.0 °C | 14000000.0 - 18000000.0 S/m Show Material materials with Electrical conductivity of 14000000.0 - 18000000.0 S/m | T5 | DIN 1725-2, EN 1676, EN 1706 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminium | 82.1 % Show Material materials with Aluminium of 82.1 % | T5 | DIN 1725-2, EN 1676, EN 1706 |
Copper | 2.0 - 3.5 % Show Material materials with Copper of 2.0 - 3.5 % | T5 | DIN 1725-2, EN 1676, EN 1706 |
Iron | 0.8 Show Material materials with Iron of 0.8 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Lead | 0.2 Show Material materials with Lead of 0.2 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Manganese | 0.1 - 0.5 % Show Material materials with Manganese of 0.1 - 0.5 % | T5 | DIN 1725-2, EN 1676, EN 1706 |
Nickel | 0.3 Show Material materials with Nickel of 0.3 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Silicon | 8.0 - 11.0 % Show Material materials with Silicon of 8.0 - 11.0 % | T5 | DIN 1725-2, EN 1676, EN 1706 |
Tin | 0.1 Show Material materials with Tin of 0.1 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Titanium | 0.15 Show Material materials with Titanium of 0.15 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Zinc | 1.2 Show Material materials with Zinc of 1.2 | T5 | DIN 1725-2, EN 1676, EN 1706 |
Technological properties
Property | ||
---|---|---|
Processing methods | permanent mould casting |