General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 10.5 g/cm³ Show Material materials with Density of 10.5 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | -195.0 °C | 89 GPa Show Material materials with Elastic modulus of 89 GPa | |
20.0 °C | 80 GPa Show Material materials with Elastic modulus of 80 GPa | ||
200.0 °C | 77 GPa Show Material materials with Elastic modulus of 77 GPa | ||
400.0 °C | 67 GPa Show Material materials with Elastic modulus of 67 GPa | ||
600.0 °C | 57 GPa Show Material materials with Elastic modulus of 57 GPa | ||
800.0 °C | 46 GPa Show Material materials with Elastic modulus of 46 GPa | ||
900.0 °C | 40 GPa Show Material materials with Elastic modulus of 40 GPa | ||
Hardness, Vickers | 20.0 °C | 70 [-] Show Material materials with Hardness, Vickers of 70 [-] | |
Poisson's ratio | 23.0 °C | 0.37 [-] Show Material materials with Poisson's ratio of 0.37 [-] | Typical for Silver |
Shear modulus | 20.0 °C | 26 GPa Show Material materials with Shear modulus of 26 GPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.79E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.79E-5 1/K | |
150.0 °C | 1.86E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.86E-5 1/K | ||
200.0 °C | 1.91E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.91E-5 1/K | ||
250.0 °C | 1.92E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.92E-5 1/K | ||
300.0 °C | 1.94E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.94E-5 1/K | ||
350.0 °C | 1.97E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.97E-5 1/K | ||
400.0 °C | 1.99E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.99E-5 1/K | ||
450.0 °C | 2.01E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.01E-5 1/K | ||
500.0 °C | 2.04E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.04E-5 1/K | ||
600.0 °C | 2.12E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.12E-5 1/K | ||
700.0 °C | 2.25E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.25E-5 1/K | ||
800.0 °C | 2.36E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.36E-5 1/K | ||
900.0 °C | 2.43E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.43E-5 1/K | ||
Melting point | 962 °C Show Material materials with Melting point of 962 °C | Typical for Silver | |
Specific heat capacity | 23.0 °C | 234 - 251 J/(kg·K) Show Material materials with Specific heat capacity of 234 - 251 J/(kg·K) | Typical for Silver |
Thermal conductivity | -233.0 °C | 1050 W/(m·K) Show Material materials with Thermal conductivity of 1050 W/(m·K) | |
-173.0 °C | 475 W/(m·K) Show Material materials with Thermal conductivity of 475 W/(m·K) | ||
-73.0 °C | 441 W/(m·K) Show Material materials with Thermal conductivity of 441 W/(m·K) | ||
20.0 °C | 419 W/(m·K) Show Material materials with Thermal conductivity of 419 W/(m·K) | ||
127.0 °C | 426 W/(m·K) Show Material materials with Thermal conductivity of 426 W/(m·K) | ||
327.0 °C | 411 W/(m·K) Show Material materials with Thermal conductivity of 411 W/(m·K) | ||
527.0 °C | 397 W/(m·K) Show Material materials with Thermal conductivity of 397 W/(m·K) | ||
927.0 °C | 383 W/(m·K) Show Material materials with Thermal conductivity of 383 W/(m·K) | ||
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 20.0 °C | 6.00E+7 S/m Show Material materials with Electrical conductivity of 6.00E+7 S/m |
Electrical resistivity | 20.0 °C | 1.67E-8 - 1.8E-8 Ω·m Show Material materials with Electrical resistivity of 1.67E-8 - 1.8E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Silver | 99.97 % Show Material materials with Silver of 99.97 % |