Properties

Mechanical

Hardness, Vickers, 5 HV 5

235 [-] at 20 °C

Yield strength Rp0.2 Rp0.2

620 MPa at 20 °C

Thermal

Melting point Tm

970 °C

Chemical properties

Element

Weight %

Comment

Au

70 %

Ag

13.5 %

Cu

8.8 %

Pt

4.4 %

Pd

2 %