Trade Name Degulor NF IV precipitation hardened (+P)

.XLSX
.PDF
Save

Properties

Mechanical

Hardness, Vickers, 5 HV 5

230 [-] at 20 °C

Yield strength Rp0.2 Rp0.2

590 MPa at 20 °C

Thermal

Melting point Tm

1100 °C

Chemical properties

Element

Weight %

Comment

Au

71 %

Pt

12.9 %

Ag

10 %

Zn

4 %

Pd

2 %

This material data has been provided by WIAM.