Iridium

Iridium (Ir)

.XLSX
.PDF
Save

Properties

Electrical

Electrical resistivity ρel

4.7E-8 Ω·m 0

Show chart

General

Density ρ

22.4 g/cm³ at 20 °C

Mechanical

Elastic modulus E

560 GPa at -180 °C

Show chart

Elongation A

6 - 18 % at 20 °C

Hardness, Vickers HV

97 - 590 [-] at 20 °C

Tensile strength Rm

120 - 500 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

44 - 130 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

6.7E-6 1/K at 100 °C

Show chart

Melting point Tm

2447 - 2454 °C

Thermal conductivity λ

149 W/(m·K) at -73 °C

Show chart

Chemical properties

Element

Weight %

Comment

Ir

99.9 %

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.