Osmium (Os)

.XLSX
.PDF
Save

Properties

Electrical

Electrical resistivity ρel

8.2E-8 Ω·m 0

Show chart

General

Density ρ

22.61 g/cm³ at 20 °C

Mechanical

Elastic modulus E

570 GPa at 20 °C

Hardness, Vickers HV

130 - 680 [-] at 20 °C

Thermal

Coefficient of thermal expansion α

4E-6 - 5.8E-6 1/K at 50 °C

Show chart

Melting point Tm

3050 °C

Thermal conductivity λ

93 W/(m·K) at -73 °C

Show chart

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.