Palladium

Palladium (Pd)

.XLSX
.PDF
Save

Properties

Electrical

Electrical resistivity ρel

9.9E-8 - 1.01E-7 Ω·m at 20 °C

General

Density ρ

12 g/cm³ at 20 °C

Mechanical

Elastic modulus E

126 GPa at -195 °C

Show chart

Elongation A

16 - 94 % at 20 °C

Hardness, Vickers HV

9 - 140 [-] at 20 °C

Tensile strength Rm

9 - 440 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

5 - 340 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.18E-5 1/K at 50 °C

Show chart

Melting point Tm

1552 °C

Thermal conductivity λ

76 W/(m·K) at -173 °C

Show chart

Chemical properties

Element

Weight %

Comment

Pd

99.9 %

This material data has been provided by WIAM.