Properties

Electrical

Electrical conductivity σel

2.33E+7 S/m at 20 °C

Electrical resistivity ρel

4.34E-8 Ω·m 0

Show chart

General

Density ρ

12.4 g/cm³ at 20 °C

Mechanical

Elastic modulus E

405 GPa at -190 °C

Show chart

Elongation A

9 - 19 % at 20 °C

Hardness, Vickers HV

52 - 400 [-] at 20 °C

Tensile strength Rm

40 - 880 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

30 - 100 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

8E-6 1/K at 50 °C

Show chart

Melting point Tm

1960 °C

Thermal conductivity λ

185 W/(m·K) at -173 °C

Show chart

Chemical properties

Element

Weight %

Comment

Rh

99.9 %

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.