Pd57.8Ag30.0Sn6.0In4.0ZnRu precipitation hardened (+P)

Want to keep this datasheet? Save it now in your required format

Description

Palladium-based dental alloy of type Pd57.8AG30.0Sn6.0In4.0ZnRu for metal ceramics as well as for crowns and bridges.

Related Standards

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

12.16 g/cm³

Show Material materials with Density of 12.16 g/cm³

Typical for Palladium

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

121 GPa

Show Material materials with Elastic modulus of 121 GPa

Typical for Palladium

Hardness, Vickers

20.0 °C

300 [-]

Show Material materials with Hardness, Vickers of 300 [-]

Poisson's ratio

23.0 °C

0.39 [-]

Show Material materials with Poisson's ratio of 0.39 [-]

Typical for Palladium

Shear modulus

23.0 °C

42 GPa

Show Material materials with Shear modulus of 42 GPa

Typical for Palladium

Yield strength Rp0.2

20.0 °C

650 MPa

Show Material materials with Yield strength Rp0.2 of 650 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

600.0 °C

1.52E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.52E-5 1/K

Melting point

1553 °C

Show Material materials with Melting point of 1553 °C

Typical for Palladium

Specific heat capacity

23.0 °C

236 - 248 J/(kg·K)

Show Material materials with Specific heat capacity of 236 - 248 J/(kg·K)

Typical for Palladium

Thermal conductivity

23.0 °C

60 - 76 W/(m·K)

Show Material materials with Thermal conductivity of 60 - 76 W/(m·K)

Typical for Palladium

Chemical properties

PropertyValue

Indium

4 %

Show Material materials with Indium of 4 %

Palladium

57.8 %

Show Material materials with Palladium of 57.8 %

Silver

30 %

Show Material materials with Silver of 30 %

Tin

6 %

Show Material materials with Tin of 6 %

Zinc

2 %

Show Material materials with Zinc of 2 %