Tantalum (Ta) soft annealed (+A) Seamless Tube

.XLSX
.PDF
Save

Description

Primary standard name

Properties

Mechanical

Elastic modulus E

172 - 180 GPa at 20 °C

Show chart

Elongation A

30 - 35 % at 20 °C

Hardness, Vickers HV

125 [-] at 20 °C

Tensile strength Rm

160 - 280 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

70 - 200 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Nb

0.04 %

W

0.03 %

Fe

0.01 %

Mo

0.01 %

Ni

0.01 %

More

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.