Properties

Electrical

Electrical conductivity σel

7.70E+6 S/m at 20 °C

Electrical resistivity ρel

1.3E-7 Ω·m at 20 °C

General

Density ρ

7.85 g/cm³ at 20 °C

Mechanical

Elastic modulus E

210 GPa at 20 °C

Tensile strength Rm

530 MPa at 20 °C

Yield strength YS

430 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.05E-5 1/K at 20 °C

Specific heat capacity cp

465 J/(kg·K) at 20 °C

Thermal conductivity λ

55 W/(m·K) at 20 °C

This material data has been provided by Wickeder Westfalenstahl GmbH (Wickeder Group).

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.