Electrical

Electrical conductivity σel

5.00E+6 S/m at 20 °C

General

Density ρ

7.85 g/cm³ at 20 °C

Mechanical

Elastic modulus E

210 GPa at 20 °C

Tensile strength Rm

613 MPa at 20 °C

Yield strength YS

410 MPa at 20 °C

Thermal

Specific heat capacity cp

500 J/(kg·K) at 20 °C

Thermal conductivity λ

54 W/(m·K) at 20 °C