General
Property | Value | Related Standards | Shape |
---|---|---|---|
Density | 2.68 g/cm³ Show Material materials with Density of 2.68 g/cm³ | EN 573-3 | Strip, Sheet, Plate |
2.68 g/cm³ Show Material materials with Density of 2.68 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 69.0 GPa Show Material materials with Elastic modulus of 69.0 GPa | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 4000 Series Aluminium |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 4000 Series Aluminium |
Shear modulus | 26.0 GPa Show Material materials with Shear modulus of 26.0 GPa | Typical for Wrought 4000 Series Aluminium |
Tensile strength | 110.0 MPa Show Material materials with Tensile strength of 110.0 MPa | |
Yield strength | 70.0 MPa Show Material materials with Yield strength of 70.0 MPa |
Thermal
Property | Temperature | Value | Related Standards | Shape |
---|---|---|---|---|
Coefficient of thermal expansion | 2.1600000000000003e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.1600000000000003e-05 1/K | |||
20 °C | 2.16e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.16e-05 1/K | EN 573-3 | Strip, Sheet, Plate | |
100 °C | 2.16e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.16e-05 1/K | EN 573-3 | Strip, Sheet, Plate | |
Melting point | 575.0 - 615.0 °C Show Material materials with Melting point of 575.0 - 615.0 °C | EN 573-3 | Strip, Sheet, Plate | |
Specific heat capacity | 890.0 J/(kg·K) Show Material materials with Specific heat capacity of 890.0 J/(kg·K) | |||
Thermal conductivity | 180 W/(m·K) Show Material materials with Thermal conductivity of 180 W/(m·K) | EN 573-3 | Strip, Sheet, Plate | |
180.0 W/(m·K) Show Material materials with Thermal conductivity of 180.0 W/(m·K) |
Electrical
Property | Value | Related Standards | Shape |
---|---|---|---|
Electrical conductivity | 27000000.0 S/m Show Material materials with Electrical conductivity of 27000000.0 S/m | EN 573-3 | Strip, Sheet, Plate |
Electrical resistivity | 3.7e-08 Ω·m Show Material materials with Electrical resistivity of 3.7e-08 Ω·m | EN 573-3 | Strip, Sheet, Plate |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Copper | 0.25 % Show Material materials with Copper of 0.25 % | EN 573-3 | Strip, Sheet, Plate |
Iron | 0.8 % Show Material materials with Iron of 0.8 % | EN 573-3 | |
0.80 % Show Material materials with Iron of 0.80 % | EN 573-3 | Strip, Sheet, Plate | |
Manganese | 0.1 % Show Material materials with Manganese of 0.1 % | EN 573-3 | Strip, Sheet, Plate |
Silicon | 6.8 - 8.2 % Show Material materials with Silicon of 6.8 - 8.2 % | EN 573-3 | Strip, Sheet, Plate |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % | EN 573-3 | Strip, Sheet, Plate |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |