General
Property | Value |
---|---|
Density | 2.69 g/cm³ Show Material materials with Density of 2.69 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 69.0 GPa Show Material materials with Elastic modulus of 69.0 GPa | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 5000 Series Aluminium |
Shear modulus | 26.0 - 26.5 GPa Show Material materials with Shear modulus of 26.0 - 26.5 GPa | Typical for Wrought 5000 Series Aluminium |
Tensile strength | 115.0 MPa Show Material materials with Tensile strength of 115.0 MPa | |
Yield strength | 80.0 MPa Show Material materials with Yield strength of 80.0 MPa |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 2.3800000000000003e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.3800000000000003e-05 1/K | |
Max service temperature | 150.0 °C Show Material materials with Max service temperature of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Melting point | 560.0 - 655.0 °C Show Material materials with Melting point of 560.0 - 655.0 °C | Typical for Wrought 5000 Series Aluminium |
Specific heat capacity | 897.0 J/(kg·K) Show Material materials with Specific heat capacity of 897.0 J/(kg·K) | |
Thermal conductivity | 185.0 W/(m·K) Show Material materials with Thermal conductivity of 185.0 W/(m·K) |
Electrical
Property | Value | Comment |
---|---|---|
Electrical conductivity | 18000000.0 - 31000000.0 S/m Show Material materials with Electrical conductivity of 18000000.0 - 31000000.0 S/m | Typical for Wrought 5000 Series Aluminium |
Electrical resistivity | 3.3e-08 - 5e-08 Ω·m Show Material materials with Electrical resistivity of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |