General
Property | Value |
---|---|
Density | 4.51 g/cm³ Show Material materials with Density of 4.51 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 105.0 GPa Show Material materials with Elastic modulus of 105.0 GPa | |
Poisson's ratio | 0.361 [-] Show Material materials with Poisson's ratio of 0.361 [-] | Typical for Pure Titanium |
Shear modulus | 46.0 GPa Show Material materials with Shear modulus of 46.0 GPa | Typical for Pure Titanium |
Tensile strength | 315.0 MPa Show Material materials with Tensile strength of 315.0 MPa | |
Yield strength | 180.0 MPa Show Material materials with Yield strength of 180.0 MPa |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 8.7e-06 1/K Show Material materials with Coefficient of thermal expansion of 8.7e-06 1/K | |
Melting point | 1670.0 °C Show Material materials with Melting point of 1670.0 °C | Typical for Pure Titanium |
Specific heat capacity | 520.0 J/(kg·K) Show Material materials with Specific heat capacity of 520.0 J/(kg·K) | |
Thermal conductivity | 21.8 W/(m·K) Show Material materials with Thermal conductivity of 21.8 W/(m·K) |