General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.71 g/cm³ Show Material materials with Density of 8.71 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 137.68 GPa Show Material materials with Elastic modulus of 137.68 GPa |
Tensile strength | 23.0 °C | 293.6 MPa Show Material materials with Tensile strength of 293.6 MPa |
Yield strength | 23.0 °C | 151.2 MPa Show Material materials with Yield strength of 151.2 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.71E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.71E-5 1/K |
Coefficient of thermal expansion, transverse | 23.0 °C | 0.02 1/K Show Material materials with Coefficient of thermal expansion, transverse of 0.02 1/K |
Specific heat capacity | 23.0 °C | 417.35 J/(kg·K) Show Material materials with Specific heat capacity of 417.35 J/(kg·K) |
Thermal conductivity | 23.0 °C | 302.28 W/(m·K) Show Material materials with Thermal conductivity of 302.28 W/(m·K) |
Thermal conductivity, through-plane | 23.0 °C | 55.76 W/(m·K) Show Material materials with Thermal conductivity, through-plane of 55.76 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 4.36E+7 S/m Show Material materials with Electrical conductivity of 4.36E+7 S/m |
Electrical conductivity, transverse | 23.0 °C | 1.73E+7 S/m Show Material materials with Electrical conductivity, transverse of 1.73E+7 S/m |
Electrical resistivity | 23.0 °C | 2.3E-8 Ω·m Show Material materials with Electrical resistivity of 2.3E-8 Ω·m |
Technological properties
Property | ||
---|---|---|
Coating | Different coating layers are available upon request. |