General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 3.33 g/cm³ Show Material materials with Density of 3.33 g/cm³ |
Mechanical
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.24E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.24E-5 1/K |
Coefficient of thermal expansion, transverse | 23.0 °C | 0.02 1/K Show Material materials with Coefficient of thermal expansion, transverse of 0.02 1/K |
Specific heat capacity | 23.0 °C | 760.05 J/(kg·K) Show Material materials with Specific heat capacity of 760.05 J/(kg·K) |
Thermal conductivity | 23.0 °C | 238.3 W/(m·K) Show Material materials with Thermal conductivity of 238.3 W/(m·K) |
Thermal conductivity, through-plane | 23.0 °C | 231.15 W/(m·K) Show Material materials with Thermal conductivity, through-plane of 231.15 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 3.77E+7 S/m Show Material materials with Electrical conductivity of 3.77E+7 S/m |
Electrical conductivity, transverse | 23.0 °C | 2.28E+7 S/m Show Material materials with Electrical conductivity, transverse of 2.28E+7 S/m |
Electrical resistivity | 23.0 °C | 2.7E-8 Ω·m Show Material materials with Electrical resistivity of 2.7E-8 Ω·m |
Technological properties
Property | ||
---|---|---|
Coating | Different coating layers are available upon request. |