General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.19 g/cm³ Show Material materials with Density of 8.19 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 176.5 GPa Show Material materials with Elastic modulus of 176.5 GPa |
Tensile strength | 23.0 °C | 336.25 MPa Show Material materials with Tensile strength of 336.25 MPa |
Yield strength | 23.0 °C | 212.25 MPa Show Material materials with Yield strength of 212.25 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.23E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.23E-5 1/K |
Coefficient of thermal expansion, transverse | 23.0 °C | 0.01 1/K Show Material materials with Coefficient of thermal expansion, transverse of 0.01 1/K |
Specific heat capacity | 23.0 °C | 431.83 J/(kg·K) Show Material materials with Specific heat capacity of 431.83 J/(kg·K) |
Thermal conductivity | 23.0 °C | 62 W/(m·K) Show Material materials with Thermal conductivity of 62 W/(m·K) |
Thermal conductivity, through-plane | 23.0 °C | 60.66 W/(m·K) Show Material materials with Thermal conductivity, through-plane of 60.66 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 8.45E+6 S/m Show Material materials with Electrical conductivity of 8.45E+6 S/m |
Electrical conductivity, transverse | 23.0 °C | 1.31E+7 S/m Show Material materials with Electrical conductivity, transverse of 1.31E+7 S/m |
Electrical resistivity | 23.0 °C | 1.18E-7 Ω·m Show Material materials with Electrical resistivity of 1.18E-7 Ω·m |
Technological properties
Property | ||
---|---|---|
Coating | Different coating layers are available upon request. |