CuZn37 / DD14 / CuZn37 (10-80-10)

Alternative and trade names
BRAFER
.XLSX
.PDF
Save

Description

Clad material. Check out the clad configurator https://app.wickeder.de for more variants.

Related Standards

Properties

Electrical

Electrical conductivity σel

9.52E+6 S/m at 20 °C

Electrical conductivity, transverse σel, trans

1.22E+7 S/m at 20 °C

Electrical resistivity ρel

1.05E-7 Ω·m at 20 °C

General

Density ρ

7.97 g/cm³ at 20 °C

Mechanical

Elastic modulus E

188.4 GPa at 20 °C

Tensile strength Rm

318 MPa at 20 °C

Yield strength YS

190 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.1493E-5 1/K at 20 °C

Coefficient of thermal expansion, transverse αtrans

0.03 1/K at 20 °C

Specific heat capacity cp

446.36 J/(kg·K) at 20 °C

Thermal conductivity λ

68 W/(m·K) at 20 °C

Thermal conductivity, transverse λtrans

61.68 W/(m·K) at 20 °C

Technological properties

Coating

Different coating layers are available upon request.

This material data has been provided by Wickeder Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.