Nature Alu

About Nature Alu

High Purity Aluminium Producer. A company committed to sustainable development, Nature Alu's mission is to produce high-purity aluminium (P0101 up to 4N+) while respecting the environment and the health and safety good practices for their employees. The company offers a world-class environmentally friendly product, with a very low carbon footprint and is adapted to the needs of their clients.

Company profile

Headquarters

La Baie (Quebec), Canada

Revenue

0-1M USD

Number of employees

11-50

Year founded

2016

Type

Manufacturer

Processing capabilities

Aluminium purification or refining

Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

DIN Al99.99

Sow, Ingot

DIN Al99.99, High purity aluminium 3N8

P1020

Sow, Ingot

P1020, DIN Al99.97