About Asap texas

AeroSpace Aluminum Products, established in 1981, produces quality aluminum extrusions for the aerospace and military industries, as well as commercial and other applications. ASAP specializes in custom, hard alloy, short run aluminum extrusions

Company profile

Headquarters

Dike,Texas, United States

Type

Manufacturer and Processor

Certifications

AS 9100

Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

EN AW-2014

Extrusion

EN AW-2014

MIL-I-45208A, AMS 2772

EN AW-2024

Extrusion

EN AW-2024

MIL-I-45208A, AMS 2772

EN AW-2219

Extrusion

EN AW-2219

MIL-I-45208A, AMS 2772

EN AW-6061

Extrusion

EN AW-6061

MIL-I-45208A, AMS 2772

EN AW-7050

Extrusion

EN AW-7050

MIL-I-45208A, AMS 2772

EN AW-7075

Extrusion

EN AW-7075

MIL-I-45208A, AMS 2772

EN AW-7178

Extrusion

EN AW-7178

MIL-I-45208A, AMS 2772

Locations

United States

United States

5834 Farm Road 71 E

75437 Dike,Texas

(+1)9039453668