Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

EN DC01

Strip

EN DC01, EN 1.0330

DIN EN 10139

EN DC03

Strip

EN DC03, EN 1.0347

DIN EN 10139

EN DC04

Strip

EN DC04, EN 1.0338

DIN EN 10139

EN DC05

Strip

EN DC05, EN 1.0312

DIN EN 10139

EN DC06

Strip

EN DC06, EN 1.0873

DIN EN 10139

EN ZE500

Strip

EN ZE500, EN 1.0489

EN 10268

EN ZE550

Strip

EN ZE550, EN 1.0489

EN 10268

EN ZE600

Strip

EN ZE600, EN 1.0548

EN 10268

EN ZE650

Strip

EN ZE650, EN 1.0550

EN 10268

EN ZE700

Strip

EN ZE700, EN 1.0550

EN 10268