activity focuses on the processing of stainless steels, particularly special steels and clad materials, to create "tailor-made product solution
Headquarters
Gifhorner,Lower Saxony, Germany
Website
Type
Processor
Certifications
ISO 9001
, ISO 14001
, ISO 45001
, EN 1090-2
, KTA 3211.1
, KTA 3211.3
, KTA 1408.3
, NADCAP
, ISO 50001
, KTA 1401
, AD 2000
, AS 9100
, DGRL 2014/68/EU
, DGRL 2014/68/EU
, DIN 2303
, IEC 17025
, ISO 17025
, ISO 3834
Grade | Shape | ||
---|---|---|---|
ASTM TP304L | Pipe, Tube | ASTM TP304L | ASTM A312, ASTM A358 |
ASTM TP316L | Pipe, Tube | ASTM TP316L | ASTM A312, ASTM A358 |
DIN 1.4307 | Pipe, Tube | DIN 1.4307 | DIN EN 10217-7 |
DIN 1.4404 | Pipe, Tube | DIN 1.4404 | DIN EN 10217-7 |
DIN 1.4410 | Pipe, Tube | DIN 1.4410, UNS S32750, Alloy 2507 | ASTM A928 |
DIN 1.4462 | Pipe, Tube | DIN 1.4462, UNS S32205, Alloy 2205 | ASTM A790, ASTM A928 |
DIN 1.4539 | Pipe, Tube | DIN 1.4539 | DIN EN 10217-7 |
DIN 1.4541 | Pipe, Tube | DIN 1.4541 | DIN EN 10217-7 |
DIN 1.4571 | Pipe, Tube | DIN 1.4571 | DIN EN 10217-7 |