EMJ is a leading supplier of Steel and Aluminum Bar, Tubing, and Plate to manufacturing companies in North America and around the world. Our broad network of facilities, superior inventories, extensive value-added processing capabilities,
Headquarters
Lynwood,California, United States
Website
Type
Manufacturer and Processor
Certifications
AS 9120B
, ISO 9001
Grade | Shape | ||
---|---|---|---|
AISI 4130 | Bar | AISI 4130, UNS G41300 | AMS S6758, AMS 6370, AMS 2301 |
AISI 4140 | Bar | AISI 4140, UNS G41400 | |
AISI 4330 | Bar | AISI 4330 | AMS 6411, AMS 6427, AMS 2300 |
AISI 4340 mod. | Bar | AISI 4340 mod. | AMS 6417, AMS 2300 |
AISI 4620 | Bar | AISI 4620, UNS G46200 | AMS 6294, AMS 2301 |
AISI 9310 | Bar | AISI 9310, UNS G93106 | MIL-S-7393, AMS 6260, AMS 2301 |
AISI E4340 | Bar | AISI E4340, UNS G43406 | |
AISI E52100 | Bar | AISI E52100, UNS G15216, UNS G52986 | AMS S7420, AMS 6440, AMS 2301, ASTM A295 |