Rosen Metall - your professional partner for non-ferrous metals, stainless steel and plastics in the Euregio Aachen. As a stockist, regional full-range supplier, we stock the most important dimensions for all metal consumers for speedy delivery with our vehicle fleet within the Euregio Aachen.
Headquarters
Eilendorf, Germany
Website
Type
Processor and Distributor
Grade | Shape | ||
---|---|---|---|
EN AW-1050A | Sheet, Pipe, Tube, Plate, Rod, Profile, Fitting | EN AW-1050A, EN Al99.5, DIN 3.0255 | |
EN AW-2007 | Sheet, Pipe, Tube, Plate, Rod, Profile, Fitting | EN AW-2007, DIN 3.1645, DIN AlCuMgPb | |
EN AW-2011 | Sheet, Pipe, Tube, Plate, Rod, Profile, Fitting | EN AW-2011, DIN 3.1655, DIN AlCu6BiPb(A) | |
EN X14CrMoS17 | Sheet, Plate, Rod, Profile, Tube, Fitting | EN X14CrMoS17, EN 1.4104 | EN 10088 |
EN X17CrNi16-2 | Sheet, Plate, Rod, Profile, Tube, Fitting | EN X17CrNi16-2, EN 1.4057 | EN 10088 |
EN X20Cr13 | Sheet, Plate, Rod, Profile, Tube, Fitting | EN X20Cr13, EN 1.4021 | EN 10088 |
EN X2CrNiMo17-12-2 | Sheet, Plate, Rod, Profile, Tube, Fitting | EN X2CrNiMo17-12-2, EN 1.4404 | EN 10088 |
EN X39CrMo17-1 | Sheet, Plate, Rod, Profile, Tube, Fitting | EN X39CrMo17-1, EN 1.4122 | EN 10088 |
EN X46Cr13 | Sheet, Plate, Rod, Profile, Tube, Fitting | EN X46Cr13, EN 1.4034 | EN 10088 |
EN X90CrMoV18 | Sheet, Plate, Rod, Profile, Tube, Fitting | EN X90CrMoV18, EN 1.4112 | EN 10088 |